JavaScript is disabled for your browser. Some features of this site may not work without it.

    Listar

    Todo RIUMAComunidades & ColeccionesPor fecha de publicaciónAutoresTítulosMateriasTipo de publicaciónCentrosDepartamentos/InstitutosEditoresEsta colecciónPor fecha de publicaciónAutoresTítulosMateriasTipo de publicaciónCentrosDepartamentos/InstitutosEditores

    Mi cuenta

    AccederRegistro

    Estadísticas

    Ver Estadísticas de uso

    DE INTERÉS

    Datos de investigaciónReglamento de ciencia abierta de la UMAPolítica de RIUMAPolitica de datos de investigación en RIUMAOpen Policy Finder (antes Sherpa-Romeo)Dulcinea
    Preguntas frecuentesManual de usoContacto/Sugerencias
    Ver ítem 
    •   RIUMA Principal
    • Investigación
    • Artículos
    • Ver ítem
    •   RIUMA Principal
    • Investigación
    • Artículos
    • Ver ítem

    Valorization of furfural to obtain high value-sdded products with ZrO2- and Al2O3-Pillared clays

    • Autor
      Es Sih, Salima; Franco-Duro, Francisco IgnacioAutoridad Universidad de Málaga; García-Sancho, CristinaAutoridad Universidad de Málaga; García-Mateos, Francisco JoséAutoridad Universidad de Málaga; Rosas-Martínez, Juana MaríaAutoridad Universidad de Málaga; Moreno-Tost, RamónAutoridad Universidad de Málaga; Maireles-Torres, Pedro JesúsAutoridad Universidad de Málaga; Cecilia-Buenestado, Juan AntonioAutoridad Universidad de Málaga
    • Fecha
      2024
    • Editorial/Editor
      Springer
    • Palabras clave
      Aldehídos - Reactividad; Filosilicatos - Reactividad
    • Resumen
      Two phyllosilicates (montmorillonite and saponite) have been selected as starting materials to synthesize ZrO2- and Al2O3-pillared clays by the insertion of polyoxocations and subsequent calcination. These pillared clays display higher surface area, porosity and available acid sites in comparison to their respective raw clays. These samples were tested in the one-pot process to transform furfural into obtain valuable products. The incorporation of ZrO2 allows to reach the highest furfural conversion values, with high yields towards furfuryl alcohol (FOL) at shorter reaction times, whereas the formation of i-propyl furfuryl ether (iPFE) is favored at longer times, attaining iPFE yields of about 50% after 24 h at 170 ºC, using isopropanol as sacrificing alcohol.
    • URI
      https://hdl.handle.net/10630/31429
    • DOI
      https://dx.doi.org/https://doi.org/10.1007/s11244-024-01971-3
    • Compartir
      RefworksMendeley
    Mostrar el registro completo del ítem
    Ficheros
    s11244-024-01971-3.pdf (5.343Mb)
    Colecciones
    • Artículos

    Estadísticas

    REPOSITORIO INSTITUCIONAL UNIVERSIDAD DE MÁLAGA
    REPOSITORIO INSTITUCIONAL UNIVERSIDAD DE MÁLAGA
     

     

    REPOSITORIO INSTITUCIONAL UNIVERSIDAD DE MÁLAGA
    REPOSITORIO INSTITUCIONAL UNIVERSIDAD DE MÁLAGA